Preparation of long afterglow luminescent flame retardant coatings

Preparation method The components except the long-afterglow luminous powder are mixed evenly with a stirring device, and then the long-afterglow luminous powder is added in the case of slow stirring, stirring for a period of time and then quickly stirring until uniform. Raw material compatibility The mass proportion range of each component of this product: high chlorinated polyethylene (30%)20~40; Chlorinated rubber 1 ~ 5; 70% chlorinated paraffin 3~8; 50% chlorinated paraffin 2 to 6; Antimony trioxide 2~5; Dispersant 0.1 ~ 0.5; Fumed...