A making method of rare earth photoluminescence safety paint
Raw material: Styrene-acrylic emulsion,rutile titanium dioxide,talcum powder,mica powder,luminous pigment,glycol pigment dispersant (agent),defoamer,Thickener Preparation method Firstly, measure the emulsion, and then put a certain amount of styrene-acrylic emulsion into a beaker; Then, all kinds of additives are measured separately, and then the additives except defoamer are put into another beaker, fully stirred and mixed into mixed additives; Add defoamer into the mixed additives, mix evenly, slowly add people into half of the emulsion, and continue to stir for 10min for later use; Putting the...