Application of luminescent powder in printing paste
The preparation and application methods of luminous printing paste described in this paper are for reference only, and corresponding adjustments should be made in practical application. Select medium-sized or alkaline transparent printing paste and D-type or S-type luminescent pigment with the weight ratio of 20-50%, and mix them evenly.
Adjust the viscosity with the corresponding diluent. Before printing luminescent printing paste, you should first lay a layer of white background.
The following transparent printing pastes are available for selection.
Nylon printing paste
Advanced printing paste
High elastic transparent printing paste
High gloss printing paste
Nylon transparent printing paste
Formula example
Luminous pigment 25g Japanese transparent printing paste 20g viscous 30g thickener 3g auxiliary 10g.
Total soft water 12g: 100g
Physical characteristics of luminous printing paste
Appearance: light gray, foamy.
Components: Alkaline aluminate and acrylate.
Viscosity: 60000 CPS
Pb: 7-8
Ionic characteristics: anions
Luminous color: yellow green or blue green
manufacturing technique
Printing-Drying-Secondary Printing-Drying-Pressing (140℃ for 10 seconds)/Drying (140℃ for 3 minutes)